Fix

Why epoxy resin stays sticky and how to fix a bad cure

Published

As an Amazon Associate we earn from qualifying purchases. This does not change our picks. Affiliate disclosure
New to Prime? Try Prime free for fast, free shipping on eligible items.

Gear for this job

All 7 picks compared
Closeup of an artisan using a blowtorch to work on epoxy resin in a workshop
Photo: Collab Media on Pexels

This page is for two-part epoxy: coating, casting and deep pour resins mixed from Part A and Part B. Coating and casting epoxies are usually hard to the touch in about 24 hours and fully cured in 72 hours at 70 to 77 F. Deep pour resins can need 24 to 72 hours before demolding and 5 to 7 days for a full cure, so check the label before calling a cure failed. What decides the fix is how the surface feels: liquid, tacky like tape, or hard with a few soft spots. One-part UV resin fails for different reasons, covered in why UV resin stays sticky.

What kind of sticky is it?

Press a gloved fingertip on the surface and compare it with the rows below. The three main cases follow ArtResin's troubleshooting guide for sticky resin, and each one has a different fix. Wait for the cure time on your own label before testing: a deep pour resin can still be soft at 24 hours and be fine.

Why is my epoxy resin not hardening at all?

Resin that is still liquid, runny or gooey well past the cure time on the label was almost always measured wrong. The usual versions: unequal amounts of a 1:1 resin, a by-volume resin measured on a scale, or two pours from the same bottle. Part A is denser than Part B, so 1:1 by volume is never 1:1 by weight. ArtResin, for example, is 1:1 by volume but 100:84 by weight, and its maker says to measure by volume.

Waiting does not correct a wrong ratio, and extra hardener does not speed a cure. Data sheets say an off ratio leaves the resin tacky or uncured. ArtResin's fix for liquid resin is to scrape off as much as possible, then pour a fresh coat that is measured and mixed correctly. Check the ratio and the basis (volume or weight) on your label, then let the mixing ratio calculator split the batch into Part A and Part B.

Why is my resin art sticky all over?

A surface that feels like the sticky side of tape, with no wet patches, points to a slow or incomplete cure. ArtResin lists three causes: a room below the ideal range, slightly inaccurate measuring, or under-mixing. Makers ask for a steady room of about 70 to 80 F. ArtResin asks for 75 to 85 F and reports trouble below 72 F, TotalBoat gives 65 to 80 F and MAS gives 60 to 75 F for its deep pour resin, so read your own label.

Cold slows the reaction. As a rule of thumb only, each 18 F (10 C) cooler roughly doubles pot life and cure time, so a piece in a cold garage can need far longer than the label says. ArtResin's fix is to move the piece to a warmer spot for 24 hours. If it is still tacky after that, pour a fresh, carefully measured coat straight over it. A tacky surface does not need scraping first. The epoxy cure time chart lists normal times by resin type.

Note.Keep the room temperature steady for the first 24 hours of the cure. ArtResin names that window as the one that matters. A room that cools overnight can leave a tacky finish.

How to fix sticky spots in epoxy resin

Random soft or wet spots on an otherwise hard surface come from unmixed resin. Resin and hardener cling to the sides and bottom of the cup, and scraping the cup out while pouring drops that unmixed material onto the piece. The cured part is fine. Only the spots need work before a new coat goes on.

  1. 1

    Put on nitrile gloves and scrape every wet or gummy spot out with a plastic scraper or craft stick. Wipe away the residue with a paper towel.

  2. 2

    Sand the whole cured surface with 80 grit sandpaper so the new coat can grip. ArtResin names 80 grit for this job. Wear a particulate mask for the dust.

  3. 3

    Remove all sanding dust with a damp cloth and let the surface dry completely. Moisture under a new coat causes cloudy areas.

  4. 4

    Measure a fresh batch the way the label says and stir slowly for 3 to 5 minutes, scraping the sides and bottom. Pour a full coat over the whole surface, not only the patches.

  5. 5

    Leave the piece in a steady room of 70 to 80 F, or the range on your label, for the full cure time. Most coating epoxies are hard in about 24 hours and fully cured in 72 hours.

Can too much colorant stop epoxy from curing?

Yes. Colorant is not part of the resin chemistry, so every drop dilutes the mix. ArtResin's limit is 6 percent of the total volume of mixed resin and hardener, which is 6 ml in a 100 ml batch. Past the limit the resin can stay wet or soft, and the fix is the same as for a wrong ratio: scrape it off and recoat. Other makers set their own limits, so check the label. Colorants that contain water, and inclusions that are not fully dry, add a second problem: cloudy resin.

Why is my casting resin still sticky in the mold?

Casting and deep pour resins cure slower than coating resins by design. Typical data-sheet figures at 70 to 77 F are 18 to 24 hours to demold a casting epoxy and 24 to 72 hours for a deep pour, with a full cure in 5 to 7 days for many deep pour products. Thin castings are slower still: Smooth-On notes for its EpoxAcast resins that castings of 1/4 inch or less cure more slowly. A piece that is firm but slightly tacky at the label's demold time usually needs more time in a warm room, not a repair.

A casting that is still liquid in the mold after the full cure time has the same causes as a wet coating: ratio, mixing or too much colorant. A top coat cannot fix resin that is liquid inside a mold. Empty the mold, wipe the uncured resin off the silicone with isopropyl alcohol and pour again. If the piece is hard but flexes, that is a different symptom, covered in why cured resin is bendy.

How to prevent sticky epoxy next time

Nearly every sticky cure traces back to measuring, mixing or temperature, so the prevention list is short. The maker's instructions win wherever they differ from these general figures.

  • Measure the way the label says, by volume or by weight, and never swap one for the other. Size the batch with the resin calculator first.
  • Stir slowly for 3 to 5 minutes, scraping the sides and bottom of the cup. ArtResin asks for at least 3 minutes.
  • Several makers ask for a second cup: pour the mix into a clean cup and stir again. Smooth-On specifies this for EpoxAcast 690.
  • Do not scrape the cup out onto the piece. What clings to the walls is the least mixed resin in the batch.
  • Keep colorant under the maker's limit, which is 6 percent of the mixed volume for ArtResin.
  • Hold the room at about 70 to 80 F, or your label's range, for at least the first 24 hours. Warm cold bottles, caps closed, in warm water for 10 to 15 minutes before measuring.

Quick answers

Short answers to the questions asked most about sticky epoxy. Figures come from maker instructions and data sheets, and your own label has the final word.

  • How to fix sticky epoxy resin? If it is only tacky, give it 24 hours in a warm room, then pour a fresh coat over it. If it is wet, scrape it off first.
  • Why is my resin soft? Soft spots come from unmixed resin scraped out of the cup. A piece that is soft or bendy all over was demolded early, is thin, or was mixed off ratio.
  • Why is my epoxy resin not hardening? A wrong ratio, a by-volume resin measured on a scale, too much colorant or short mixing. Scrape off the liquid resin and recoat.
  • Why is my casting resin still sticky? Casting and deep pour resins need 18 to 72 hours before demolding, longer in a cold room. Check the label, then add warmth and time.
  • How to fix epoxy resin that didn't cure? Scrape off everything wet, sand the cured areas with 80 grit, wipe clean and pour a new, correctly measured coat.

What you need for this

Sources