# Epoxy resin cure time chart: by room temperature and resin type

Source: https://resinandmold.com/blog/epoxy-resin-cure-time-chart
Published: 2026-10-01
Publisher: Resin and Mold

**Short answer:** At 70 to 77 F, coating and casting epoxies are hard enough to demold in about 18 to 24 hours and fully cured in 72 hours. Deep pour epoxies need 24 to 72 hours before demolding and 5 to 7 days for a full cure, some 7 to 14. A colder room stretches every figure, so the label on your bottle has the final word.

Cure time is not one number. Every data sheet gives a working time (how long the mix stays pourable), a demold or hard time and a full cure, each measured at a set temperature, usually 70 to 77 F, for a stated mass or depth. This chart puts those figures side by side for the three types of two-part epoxy and for named products, with the document each row comes from. It covers epoxy only. One-part UV resin is on the [UV resin curing time chart](https://resinandmold.com/blog/uv-resin-curing-time-chart).

## Epoxy resin cure time chart by resin type and product

The first three rows are typical ranges for each resin type. The rows under them are single products, taken from the maker's technical data sheet or product page. Times apply at the temperature and pour size in the last column. Where your label differs, follow the label.

| Resin | Working time | Demold or hard | Full cure | Measured at |
| --- | --- | --- | --- | --- |
| Coating or art epoxy (typical) | 40 to 60 min | about 24 h | 72 h | 70 to 77 F, layers of about 1/8 in |
| Casting epoxy (typical) | 30 min to 5 h | 18 to 24 h | 72 h | 70 to 77 F, up to 3/8 in per layer |
| Deep pour epoxy (typical) | 30 min to 12 h, by brand | 24 to 72 h | 5 to 7 days, some 7 to 14 | 70 to 77 F, 1 to 2 in, label decides |
| ArtResin (coating) | 40 to 60 min | touch dry 5 to 8 h, hard cure 24 h | 72 h | 72 to 77 F. ArtResin data sheet, May 2018 |
| Alumilite Amazing Clear Cast (casting and coating) | 45 to 60 min | demold 18 to 24 h | 72 h | 75 F, 100 g mass. Alumilite data sheet, 12/2020 |
| Let's Resin casting epoxy | 40 to 50 min | demold 8 to 24 h | 2 to 3 days | Room of 75 to 85 F. Let's Resin support page |
| Smooth-On EpoxAcast 690 (casting) | pot life 5 h | cure time 24 h | not listed separately | 70 F, 3/8 in thick. Smooth-On technical bulletin |
| Alumilite Amazing Deep Pour | 60 to 90 min | demold 24 to 72 h | 5 to 7 days | Temperature not stated. Maker data on a retailer page |
| TotalBoat ThickSet (deep pour) | 10 to 30 min listed, gel time 5.5 h | tack free 4 to 8 h, sandable 12 to 24 h | 5 to 7 days | 77 F, 1/2 to 1 in pours. TotalBoat data sheet, 2019 |
| MAS Deep Pour | 3 h | cure time 24 to 36 h | not listed | Room of 60 to 75 F. MAS product page |
| EcoPoxy FlowCast (deep pour) | 8 to 12 h | demold 3 days | 7 to 14 days | 70 F, river table pour 1.5 in deep. EcoPoxy data sheet, 2022 |
| Smooth-On EpoxAcast 692 Deep Pour | pot life 12 h | cure time 72 h | not listed separately | 70 F, 1 1/2 in thick. Smooth-On technical bulletin |

Two-part epoxy only. Figures from maker technical data sheets and product pages, checked October 2026. Formulas change, so the product's own instructions win.

## Epoxy resin temperature chart: the room each maker asks for

No maker checked publishes a cure time for every room temperature, so this page does not invent one. Data sheets give the room range the resin is made for. Inside it, the times in the first chart apply. Below it, expect a slower cure and the risk of a tacky finish.

| Product | Room temperature the maker gives | What the maker adds |
| --- | --- | --- |
| ArtResin | 75 to 85 F ideal | The room should not fluctuate. Trouble starts below 72 F |
| Let's Resin casting epoxy | 75 to 85 F | Cold can prevent a proper cure |
| Alumilite Amazing Clear Cast | Times given at 75 F | Warmer rooms and larger batches shorten the working time |
| EcoPoxy FlowCast | 68 to 77 F, ideal 72 F | Times vary with volume, shape and mold material |
| TotalBoat ThickSet | 65 to 80 F | Required for the epoxy to cure fully |
| MAS Deep Pour | 60 to 75 F | Do not pour above 75 F: risk of yellowing and cracking |
| Smooth-On EpoxAcast 690 and 692 | 70 F | Cooler rooms recommended for large mass pours |

Room temperatures as printed in the documents named in the first chart, plus ArtResin's cold weather guidance.

## How does a cold room change epoxy cure time?

Cold slows the reaction between resin and hardener. ArtResin says curing can take much longer in cold conditions, sometimes up to several days, and can end with a sticky finish. As a rule of thumb only, not a maker figure: each **18 F (10 C)** cooler roughly doubles pot life and cure time. A piece in a cold garage can need twice the time on the label or more.

Heat works the other way: ArtResin's data sheet says curing is accelerated in a warm environment. Warmer is not always better, though. MAS says not to pour its deep pour resin above 75 F, and Smooth-On recommends cooler rooms for large mass pours.

Note: Do not add extra hardener to speed up a cure. An off ratio leaves resin tacky or uncured. Check the split with the [mixing ratio calculator](https://resinandmold.com/tools/resin-mixing-ratio-calculator).

## How long to leave resin in a silicone mold

Leave it until the demold time on the label. From the chart, that is about **18 to 24 hours** for most casting epoxies at 70 to 77 F and 24 to 72 hours for deep pour resins. Demold time is not full cure. EcoPoxy notes that a demolded casting is solid but may still sag under its own weight, and should be supported until it is fully cured.

A piece pulled early can bend or take fingerprints: see [why cured resin is bendy](https://resinandmold.com/blog/why-is-my-resin-bendy). Wait for the full cure before using a piece, and [sand and polish](https://resinandmold.com/blog/how-to-sand-and-polish-resin) only resin that has fully cured.

## How to tell when epoxy is cured

Makers describe simple checks. Smooth-On says cured material is hard and cannot be penetrated with a fingernail. EcoPoxy tests the surface with a gloved finger: set to touch means no tackiness between glove and surface. For demolding, its test is a wedge slipped under one corner of the casting with no visible bending.

If the surface is still wet well past the label's time in a room inside the maker's range, waiting will not fix it. The cause is usually ratio or mixing: see [why epoxy resin stays sticky](https://resinandmold.com/blog/epoxy-resin-still-sticky).

## Why thin or small castings take longer to cure

Data-sheet times are measured on a stated mass or depth: 100 g for Amazing Clear Cast, 3/8 in for EpoxAcast 690. Epoxy makes its own heat as it cures, and a small or thin piece makes little of it. Smooth-On says castings of 1/4 in or less cure more slowly. Let's Resin suggests 1 or 2 extra days for thin layers and small molds if needed.

Large batches go the other way. Alumilite says a batch of about 1 gallon can cut the open time in half, and pouring deeper than the label allows builds enough heat for bubbles and cracks. The [resin calculator](https://resinandmold.com/tools/resin-calculator) works out how many layers a mold needs.

## Safe ways to keep a cure warm

The aim is a steady room inside the maker's range, not extra heat on the piece. ArtResin calls the first 24 hours of the cure crucial and asks for a room that stays warm, dry and stable.

- Heat the room, not the resin surface. ArtResin suggests a space heater, or a small heated box for small projects.
- Hold the temperature overnight. A room that cools after you leave can give a tacky or uneven surface.
- Warm cold bottles before measuring: caps closed, in warm (not hot) water for 10 to 15 minutes. Working time drops by about 10 minutes.
- If a piece is only tacky after the label's time, ArtResin's advice is a warmer spot for 24 hours before calling it failed.

## Quick answers

Short answers on epoxy cure time. Figures are from maker data sheets at 70 to 77 F, and the label on your own resin has the final word.

- **How long for art resin to cure?** ArtResin's data sheet lists touch dry in 5 to 8 hours, hard cure in 24 hours and full cure in 72 hours.
- **How long does epoxy resin take to set?** Coating and casting epoxies are usually hard in about 24 hours at 70 to 77 F. Deep pour resins take 24 to 72 hours.
- **How long to leave resin in a silicone mold?** Until the label's demold time: about 18 to 24 hours for casting epoxy and 24 to 72 hours for deep pour.
- **What is the right epoxy resin cure temperature?** Most makers ask for about 70 to 80 F. ArtResin gives 75 to 85 F, TotalBoat 65 to 80 F and MAS Deep Pour 60 to 75 F.
- **What is a normal casting resin cure time?** About 18 to 24 hours to demold and 72 hours to full cure, as Alumilite lists for Amazing Clear Cast at 75 F.

## Gear guides for this topic

- https://resinandmold.com/best/best-epoxy-resin-for-molds
- https://resinandmold.com/best/best-epoxy-resin-for-tumblers
- https://resinandmold.com/best/best-resin-polishing-kit

## Sources

- [ArtResin: Technical Data Sheet (May 2018)](https://media.easycomposites.eu/datasheets/ArtResin_Technical_Data_Sheet_May2018.pdf)
- [TotalBoat: ThickSet Clear Casting Epoxy Resin Tech Data Sheet (2019)](https://doc.jamestowndistributors.com/userportal/pdfs/TotalBoat/TotalBoat_ThickSet_Epoxy_TDS_4.11.19.pdf)
- [Smooth-On: EpoxAcast 690 and 692 Deep Pour Technical Bulletin](https://www.smooth-on.com/tb/files/EPOXACAST_690_TB.pdf)